Inconel™ 601 Material Property Data Sheet
Do you need custom fasteners created with Inconel™ 601? Since our inception, Vegas Fastener Manufacturing has met every challenge of providing
Quality, Timely, Cost-effective solutions for specialty fastener applications. Every product is built to your specifications, using your prints if necessary.
Below are the technical specifications of the Inconel™ 601 Bar Stock we have available to meet your needs.
| |
Special Metals INCONEL® Alloy 601
Subcategory: Metal; Nickel Base; Superalloy
Key Words: Inconel 601, Nickel-Chromium Alloy; Werkstoff Nr. 2.4851, UNS N06601; ASME Boiler Code Section VIII; AMS 5715, AMS 5870; ASTM B166, ASTM B167, ASTM B168; DIN 17742, 17750 - 17752
| Component | Wt. % |  | | | Al | 1 - 1.7 | | | C | Max 0.1 | | | Cr | 21 - 25 | |
| | Component | Wt. % |  | | | Cu | Max 1 | | | Fe | 13 | | | Mn | Max 1 | |
| | Component | Wt. % |  | | | Ni | 58 - 63 | | S | Max 0.015 | | | Si | Max 0.5 | |
|
Material Notes: Iron content as remainder. A nickel-chromium alloy with an addition of aluminum for outstanding resistance to oxidation and other forms of high-temperature corrosion. It also has high mechanical properties at elevated temperatures. Used for industrial furnaces; heat-treating equipment such as baskets, muffles, and retorts; petrochemical and other process equipment; and gas-turbine components. Standard product forms are round, flats, forging stock, pipe, tube, plate, sheet, strip, and wire. Data provided by the manufacturer, Special Metals.
| Physical Properties | Metric | English | Comments |
|
| Density | 8.11 g/cc | 0.293 lb/inł | |
Mechanical Properties |
|
| Tensile Strength, Ultimate | 760 MPa | 110000 psi | Solution Annealed. Value at room temperature. Value at 550°C is 620 MPa. |
| Tensile Strength, Yield | 450 MPa | 65300 psi | Solution Annealed. Value at room temperature; 0.2% offset. Value at 550°C is 330 MPa. |
| Elongation at Break | 42 % | 42 % | Solution Annealed. Value at room temperature. Value at 550°C is 32%. |
Electrical Properties |
|
| Electrical Resistivity | 0.000119 ohm-cm | 0.000119 ohm-cm | |
| Magnetic Permeability | 1.003 | 1.003 | at 200 oersted (15.9 kA/m) |
| Curie Temperature | Max -196 °C | Max -321 °F | |
Thermal Properties |
|
| CTE, linear 20°C | 13.75 µm/m-°C | 7.64 µin/in-°F | 20-100°C |
| Heat Capacity | 0.448 J/g-°C | 0.107 BTU/lb-°F | |
| Thermal Conductivity | 11.2 W/m-K | 77.7 BTU-in/hr-ft˛-°F | |
| Melting Point | 1360 - 1411 °C | 2480 - 2570 °F | |
| Solidus | 1360 °C | 2480 °F | |
| Liquidus | 1411 °C | 2570 °F | |
|
|
 |
This information is provided by
MatWeb.com, The Online Materials Database and is reprinted with their permission.
Copyright 1996-2005 by Automation Creations, Inc.
The contents, results, and technical data on this page may not
be reproduced either electronically, photographically or substantively without permission from
Automation Creations, Inc and MatWeb.com. No warranty, neither expressed nor implied, is given
regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of
information from MatWeb.com.
|
 |
|