Special Metals INCONEL® Alloy C-276
Subcategory: Metal; Nickel Base; Superalloy
Key Words: ASME SB-574, SB-575, SB-619, SB-622, SB-626, Boiler Code Sections I, III, VIII, IX; Werkstoff Nr. 2.4819, Nickel-Chromium Alloy; UNS N10276; ASTM B 574, B 575, B 619, B 622, B 626, B 751; NACE MR-01-75; DIN 17744, 17750-17752
| Component | Wt. % |  | | | C | Max 0.01 | | | Co | Max 2.5 | | | Cr | 14.5 - 16.5 | | | Fe | 4 - 7 | |
| | Component | Wt. % |  | | | Mn | Max 1 | | | Mo | 15 - 17 | | | Ni | 55 | | | P | Max 0.04 | |
| | Component | Wt. % |
 | | | S | Max 0.03 | | | Si | Max 0.08 | | | V | Max 0.35 | | | W | 3 - 4.5 | |
|
Material Notes: Nickel content as remainder. A nickel-molybdenum-chromium alloy with an addition of tungsten having excellent corrosion resistance in a wide range of severe environments. The high molybdenum content makes the alloy especially resistant to pitting and crevice corrosion. The low carbon content minimizes carbide precipitation during welding to maintain corrosion resistance in as-welded structures. Used in pollution control, chemical processing, pulp and paper production, and waste treatment. Standard product forms are round, forging stock, tube, pipe, plate, sheet, strip, and wire. Data provided by the manufacturer, Special Metals.
| Physical Properties | Metric | English | Comments |
|
| Density | 8.89 g/cc | 0.321 lb/in³ | |
Mechanical Properties |
|
| Tensile Strength, Ultimate | 790 MPa | 115000 psi | Annealed. Value at room temperature. Value at 550°C is 620 MPa. |
| Tensile Strength, Yield | 415 MPa | 60200 psi | Annealed. Value at room temperature; 0.2% offset. Value at 550°C is 230 MPa. |
| Elongation at Break | 62 % | 62 % | Annealed. Value at room temperature. Value at 550°C is 60%. |
Electrical Properties |
|
| Electrical Resistivity | 0.0001229 ohm-cm | 0.0001229 ohm-cm | |
| Magnetic Permeability | 1.0002 | 1.0002 | at 200 oersted (15.9 kA/m) |
Thermal Properties |
|
| CTE, linear 20°C | 12.2 µm/m-°C | 6.78 µin/in-°F | 20-100°C |
| Heat Capacity | 0.427 J/g-°C | 0.102 BTU/lb-°F | |
| Thermal Conductivity | 9.8 W/m-K | 68 BTU-in/hr-ft²-°F | |
| Melting Point | 1325 - 1370 °C | 2420 - 2500 °F | |
| Solidus | 1325 °C | 2420 °F | |
| Liquidus | 1370 °C | 2500 °F | |
|
|
 |
This information is provided by
MatWeb.com, The Online Materials Database and is reprinted with their permission.
Copyright 1996-2005 by Automation Creations, Inc.
The contents, results, and technical data on this page may not
be reproduced either electronically, photographically or substantively without permission from
Automation Creations, Inc and MatWeb.com. No warranty, neither expressed nor implied, is given