AK Steel Austenitic Stainless Steel 321
Subcategory: Metal; Stainless Steel; T 300 Series Stainless Steel; Austenitic
Close Analogs: Iron content calculated as remainder
| Component | Wt. % |  | | | C | Max 0.08 | | | Cr | 17 - 19 | | | Fe | 65.295 - 74 | | | Mn | Max 2 | |
| | Component | Wt. % |  | | | N | Max 0.1 | | | Ni | 9 - 12 | | | P | Max 0.045 | |
| | Component | Wt. % |  |  | |
| | S | Max 0.03 | | | Si | Max 0.75 | | | Ti | Max 0.7 | |
|
Material Notes: AK Steel 321 is a stabilized austenitic stainless steel similar to Type 304 but with a titanium addition. This titanium addition reduces or prevents carbide precipitation during welding and in 427 - 816°C service. It also improves the elevated temperature properties of the alloy. AK Steel 321 provides excellent resistance to oxidation and corrosion and possesses good creep strength. It is used primarily in applications involving continuous and intermittent service temperatures within the carbide precipitation range of 427 - 816°C.Information provided by AK Steel
| Physical Properties | Metric | English | Comments |
|
| Density | 9.01 g/cc | 0.326 lb/in³ | |
Mechanical Properties |
|
| Hardness, Rockwell B | 80 | 80 | |
| Tensile Strength, Ultimate | 621 MPa | 90100 psi | |
| Tensile Strength, Yield | 276 MPa | 40000 psi | 0.2% YS |
| Elongation at Break | 45 % | 45 % | in 2 inches |
| Modulus of Elasticity | 193 GPa | 28000 ksi | tension |
| Modulus of Elasticity | 78 GPa | 11300 ksi | torsion |
Electrical Properties |
|
| Electrical Resistivity | 7.2e-005 ohm-cm | 7.2e-005 ohm-cm | |
| Magnetic Permeability | Max 1.02 | Max 1.02 | H = 200 Oersteds, Annealed |
Thermal Properties |
|
| CTE, linear 20°C | 16.6 µm/m-°C | 9.22 µin/in-°F | 0 to 100°C |
| CTE, linear 20°C | 20.2 µm/m-°C | 11.2 µin/in-°F | to 871°C |
| Heat Capacity | 0.5 J/g-°C | 0.12 BTU/lb-°F | 0°C to 100°C |
| Thermal Conductivity | 16 W/m-K | 111 BTU-in/hr-ft²-°F | 100°C |
| Thermal Conductivity | 22 W/m-K | 153 BTU-in/hr-ft²-°F | 500°C |
Processing Properties |
|
| Melt Temperature | 1371 - 1399 °C | 2500 - 2550 °F | |
|
|
 |
This information is provided by
MatWeb.com, The Online Materials Database and is reprinted with their permission.
Copyright 1996-2005 by Automation Creations, Inc.
The contents, results, and technical data on this page may not
be reproduced either electronically, photographically or substantively without permission from
Automation Creations, Inc and MatWeb.com. No warranty, neither expressed nor implied, is given