Do you need custom fasteners created with Nickel Alloy B-3? Since our inception, Vegas Fastener Group has met every challenge of providing Quality, Timely, Cost-effective solutions for specialty fastener applications. Every product is built to your specifications, using your prints if necessary.
Below are the technical specifications of the Nickel Alloy B-3 Bar Stock we have available to meet your needs.
HASTELLOY® B-3® alloy is an additional member of the nickel-molybdenum family of alloys with excellent resistance to hydrochloric acid at all concentrations and temperatures. It also withstands sulfuric, acetic, formic and phosphoric acids, and other nonoxidizing media. B-3 alloy has a special chemistry designed to achieve a level of thermal stability greatly superior to that of its predecessors, e.g. HASTELLOY B-2 alloy. B-3 alloy has excellent resistance to pitting corrosion, to stress-corrosion cracking and to knife-line and heat-affected zone attack.
|
HASTELLOY® B-3 Nickel Alloy
Key Words: HASTELLOY® B-3 Alloy, Nickel Alloy, ASTM, Case 2140, B333, B335, B366, B564, B619 and B622, B626.
Component |
Wt. % |
Nia |
65 |
Mo |
28.5 |
Cr |
1.5 |
Fe |
1.5 |
Co |
3* |
W |
3* |
Mn |
3* |
Al |
0.5* |
Ti |
0.2* |
Si |
0.1* |
C |
0.01* |
*Maximum
aAs balance
Physical Properties |
°F |
British Units |
°C |
Metric Units |
Density |
Room |
0.333 lb./in.3 |
Room |
9.22 g/cm3 |
Melting Temperature |
2500-2585 |
|
1370-1418 |
|
Mechanical Properties |
Electrical Resistivity |
Room |
53.8 microhm-in. |
Room |
137 microhm-cm |
200 |
53.9 microhm-in. |
100 |
137 microhm-cm |
400 |
54.1 microhm-in. |
200 |
137 microhm-cm |
600 |
54.3 microhm-in. |
300 |
138 microhm-cm |
800 |
54.4 microhm-in. |
400 |
138 microhm-cm |
1000 |
55.4 microhm-in. |
500 |
140 microhm-cm |
1200 |
57.5 microhm-in. |
600 |
143 microhm-cm |
1400 |
54.4 microhm-in. |
700 |
142 microhm-cm |
1600 |
52.6 microhm-in. |
800 |
132 microhm-cm |
Mean Coefficient ofThermal Expansion |
78-200 |
5.7 microinches/in.-°F |
25-100 |
10.6 x 10-6 m/m-K |
78-400 |
6.1 microinches/in.-°F |
25-200 |
11.1 x 10-6 m/m-K |
78-600 |
6.3 microinches/in.-°F |
25-300 |
11.4 x 10-6 m/m-K |
78-800 |
6.5 microinches/in.-°F |
25-400 |
11.6 x 10-6 m/m-K |
78-1000 |
6.6 microinches/in.-°F |
25-400 |
11.6 x 10-6 m/m-K |
Thermal Properties |
Thermal Conductivity |
Room |
78 Btu-in./ft.2-hr.-°F |
Room |
11.2 W/m-K |
200 |
83 Btu-in./ft.2-hr.-°F |
100 |
12.1 W/m-K |
400 |
93 Btu-in./ft.2-hr.-°F |
200 |
13.4 W/m-K |
600 |
104 Btu-in./ft.2-hr.-°F |
300 |
14.8 W/m-K |
800 |
116 Btu-in./ft.2-hr.-°F |
400 |
16.3 W/m-K |
1000 |
129 Btu-in./ft.2-hr.-°F |
500 |
17.9 W/m-K |
1200 |
142 Btu-in./ft.2-hr.-°F |
600 |
19.6 W/m-K |
Thermal Diffusivity |
Room |
4.6 x 10-3 in.2/sec. |
Room |
3.0 x 10-3cm2/s |
200 |
4.6 x 10-3 in.2/sec. |
100 |
3.0 x 10-6cm2/s |
400 |
5.4 x 10-3 in.2/sec. |
200 |
3.4 x 10-3cm2/s |
600 |
5.8 x 10-3 in.2/sec. |
300 |
3.7 x 10-3cm2/s |
800 |
6.3 x 10-3 in.2/sec. |
400 |
4.0 x 10-3cm2/s |
1000 |
6.8 x 10-3 in.2/sec. |
500 |
4.4 x 10-3cm2/s |
1200 |
7.3 x 10-3 in.2/sec. |
600 |
4.5 x 10-3cm2/s |
1400 |
7.5 x 10-3 in.2/sec. |
700 |
4.9 x 10-3cm2/s |
1600 |
7.0 x 10-3 in.2/sec. |
800 |
4.7 x 10-3cm2/s |
1800 |
7.4 x 10-3 in.2/sec. |
900 |
4.5 x 10-3cm2/s |
|
|
1000 |
4.9 x 10-3cm2/s |
Specific Heat |
Room |
0.089 Btu/lb.-°F |
Room |
373 J/kg-K |
200 |
0.092 Btu/lb.-°F |
100 |
382 J/kg-K |
400 |
0.092 Btu/lb.-°F |
200 |
409 J/kg-K |
600 |
0.102 Btu/lb.-°F |
300 |
421 J/kg-K |
800 |
0.104 Btu/lb.-°F |
400 |
431 J/kg-K |
1000 |
0.104 Btu/lb.-°F |
500 |
436 J/kg-K |
1200 |
0.112 Btu/lb.-°F |
600 |
434 J/kg-K |
|
|
References are available for this material.